Contribute youthful strength to China's "core"! Hunan vocational college students independently develop domestically produced chip cooling materials
Hunan Daily All Media Reporter Yu Rong Correspondent Zhang ChenlianThe surface modified diamond particles are loaded into a metal mold, and then the mold and copper are placed in a vacuum pressure infiltration furnace. The furnace is vacuumed and heated to around 1000 degrees Celsius, and the melted copper liquid is poured into the composite billet...
Contribute youthful strength to China's "core"! High vocational students born in the 2000s independently develop domestically produced chip cooling materials
The surface modified diamond particles are loaded into the metal mold, and then the mold and copper are placed in a vacuum pressure infiltration furnace. The furnace is vacuumed and heated to about 1000 degrees Celsius, and the melted copper liquid is poured into the composite billet...